Slabs

As mentioned before, concrete slabs need to be poured on a well-compacted base of granular soil, sand, or gravel. If settling takes place under the slab, the concrete will be left unsupported and has the potential to crack. Although you may not see what is

taking place under a slab of cured concrete (unless there is severe erosion or settling), you can tell a settling crack from a shrinkage crack by the size of the crack. Typically, if the crack exceeds one-quarter inch in width or depth, it is said to be a symptom of a structural problem. The problem is not with the concrete, although that is what you see, but rather with the settling of the material under the slab.

Structural cracking in poured concrete walls is indicated by a gap of greater than 1/8″. Again, this type of cracking is more likely a symptom of pressure against the wall than it is from the concrete failing.